ਸਿੰਟਰਡ NdFeB ਮੈਗਨੇਟ
ਸਿੰਟਰਡ NdFeB ਮੈਗਨੇਟ ਭੌਤਿਕ ਵਿਸ਼ੇਸ਼ਤਾਵਾਂ | ||||||||
ਗ੍ਰੇਡ | ਰਿਮਨੈਂਸ | Rev. Temp.- Coeff. ਦੇ ਬੀ.ਆਰ | ਜ਼ਬਰਦਸਤੀ ਫੋਰਸ | ਅੰਦਰੂਨੀ ਜਬਰਦਸਤੀ ਬਲ | Rev. Temp.- Coeff. ਦੇ Hcj | ਅਧਿਕਤਮ ਊਰਜਾ ਉਤਪਾਦ | ਅਧਿਕਤਮ ਓਪਰੇਟਿੰਗ ਤਾਪਮਾਨ | ਘਣਤਾ |
Br (KGs) | Hcb (ਤੁਸੀਂ) | Hcj (ਤੁਸੀਂ) | (BH) ਅਧਿਕਤਮ। (MGOe) | g/cm³ | ||||
N35 | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥12 | -0.58~-0.78 | 33-36 | 80℃ | 7.6 |
N38 | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥12 | -0.58~-0.78 | 36-39 | 80℃ | 7.6 |
N40 | 12.5-12.8 | -0.11~-0.12 | ≥11.5 | ≥12 | -0.58~-0.78 | 38-41 | 80℃ | 7.6 |
N42 | 12.8-13.2 | -0.11~-0.12 | ≥11.5 | ≥12 | -0.58~-0.78 | 40-43 | 80℃ | 7.6 |
N45 | 13.2-13.8 | -0.11~-0.12 | ≥11.6 | ≥12 | -0.58~-0.78 | 43-46 | 80℃ | 7.6 |
N48 | 13.8-14.2 | -0.11~-0.12 | ≥11.6 | ≥12 | -0.58~-0.78 | 46-49 | 80℃ | 7.6 |
N50 | 14.0-14.5 | -0.11~-0.12 | ≥10.0 | ≥12 | -0.58~-0.78 | 48-51 | 80℃ | 7.6 |
N52 | 14.3-14.8 | -0.11~-0.12 | ≥10.0 | ≥12 | -0.58~-0.78 | 50-53 | 80℃ | 7.6 |
N33M | 11.3-11.7 | -0.11~-0.12 | ≥10.5 | ≥14 | -0.58~-0.72 | 31-33 | 100℃ | 7.6 |
N35M | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥14 | -0.58~-0.72 | 33-36 | 100℃ | 7.6 |
N38M | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥14 | -0.58~-0.72 | 36-39 | 100℃ | 7.6 |
N40M | 12.5-12.8 | -0.11~-0.12 | ≥11.6 | ≥14 | -0.58~-0.72 | 38-41 | 100℃ | 7.6 |
N42M | 12.8-13.2 | -0.11~-0.12 | ≥12.0 | ≥14 | -0.58~-0.72 | 40-43 | 100℃ | 7.6 |
N45M | 13.2-13.8 | -0.11~-0.12 | ≥12.5 | ≥14 | -0.58~-0.72 | 43-46 | 100℃ | 7.6 |
N48M | 13.6-14.3 | -0.11~-0.12 | ≥12.9 | ≥14 | -0.58~-0.72 | 46-49 | 100℃ | 7.6 |
N50M | 14.0-14.5 | -0.11~-0.12 | ≥13.0 | ≥14 | -0.58~-0.72 | 48-51 | 100℃ | 7.6 |
N35H | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥17 | -0.58~-0.70 | 33-36 | 120℃ | 7.6 |
N38H | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥17 | -0.58~-0.70 | 36-39 | 120℃ | 7.6 |
N40H | 12.5-12.8 | -0.11~-0.12 | ≥11.6 | ≥17 | -0.58~-0.70 | 38-41 | 120℃ | 7.6 |
N42H | 12.8-13.2 | -0.11~-0.12 | ≥12.0 | ≥17 | -0.58~-0.70 | 40-43 | 120℃ | 7.6 |
N45H | 13.2-13.6 | -0.11~-0.12 | ≥12.1 | ≥17 | -0.58~-0.70 | 43-46 | 120℃ | 7.6 |
N48H | 13.7-14.3 | -0.11~-0.12 | ≥12.5 | ≥17 | -0.58~-0.70 | 46-49 | 120℃ | 7.6 |
N35SH | 11.7-12.2 | -0.11~-0.12 | ≥11.0 | ≥20 | -0.56~-0.70 | 33-36 | 150℃ | 7.6 |
N38SH | 12.2-12.5 | -0.11~-0.12 | ≥11.4 | ≥20 | -0.56~-0.70 | 36-39 | 150℃ | 7.6 |
N40SH | 12.5-12.8 | -0.11~-0.12 | ≥11.8 | ≥20 | -0.56~-0.70 | 38-41 | 150℃ | 7.6 |
N42SH | 12.8-13.2 | -0.11~-0.12 | ≥12.4 | ≥20 | -0.56~-0.70 | 40-43 | 150℃ | 7.6 |
N45SH | 13.2-13.8 | -0.11~-0.12 | ≥12.6 | ≥20 | -0.56~-0.70 | 43-46 | 150℃ | 7.6 |
N28UH | 10.2-10.8 | -0.11~-0.12 | ≥9.6 | ≥25 | -0.52~-0.70 | 26-29 | 180℃ | 7.6 |
N30UH | 10.8-11.3 | -0.11~-0.12 | ≥10.2 | ≥25 | -0.52~-0.70 | 28-31 | 180℃ | 7.6 |
N33UH | 11.3-11.7 | -0.11~-0.12 | ≥10.7 | ≥25 | -0.52~-0.70 | 31-34 | 180℃ | 7.6 |
N35UH | 11.8-12.2 | -0.11~-0.12 | ≥10.8 | ≥25 | -0.52~-0.70 | 33-36 | 180℃ | 7.6 |
N38UH | 12.2-12.5 | -0.11~-0.12 | ≥11.0 | ≥25 | -0.52~-0.70 | 36-39 | 180℃ | 7.6 |
N40UH | 12.5-12.8 | -0.11~-0.12 | ≥11.3 | ≥25 | -0.52~-0.70 | 38-41 | 180℃ | 7.6 |
N28EH | 10.4-10.9 | -0.105~-0.120 | ≥9.8 | ≥30 | -0.48~-0.70 | 26-29 | 200℃ | 7.6 |
N30EH | 10.8-11.3 | -0.105~-0.120 | ≥10.2 | ≥30 | -0.48~-0.70 | 28-31 | 200℃ | 7.6 |
N33EH | 11.3-11.7 | -0.105~-0.120 | ≥10.5 | ≥30 | -0.48~-0.70 | 31-34 | 200℃ | 7.6 |
N35EH | 11.7-12.2 | -0.105~-0.120 | ≥11.0 | ≥30 | -0.48~-0.70 | 33-36 | 200℃ | 7.6 |
N38EH | 12.2-12.5 | -0.105~-0.120 | ≥11.3 | ≥30 | -0.48~-0.70 | 36-39 | 200℃ | 7.6 |
N28AH | 10.4-10.9 | -0.105~-0.120 | ≥9.9 | ≥33 | -0.45~-0.70 | 26-29 | 230℃ | 7.6 |
N30AH | 10.8-11.3 | -0.105~-0.120 | ≥10.3 | ≥33 | -0.45~-0.70 | 28-31 | 230℃ | 7.6 |
N33AH | 11.3-11.7 | -0.105~-0.120 | ≥10.6 | ≥33 | -0.45~-0.70 | 31-34 | 230℃ | 7.6 |
ਨੋਟ: · ਕਾਰਜਸ਼ੀਲ ਤਾਪਮਾਨ 20℃±2℃ ਦੇ ਅਧੀਨ, ਚੁੰਬਕੀ ਮਾਪਦੰਡਾਂ ਅਤੇ ਭੌਤਿਕ ਵਿਸ਼ੇਸ਼ਤਾਵਾਂ ਦੀ ਜਾਂਚ ਕੀਤੀ ਜਾਂਦੀ ਹੈ, ਜਿਸ ਵਿੱਚ ਚੁੰਬਕੀ ਬਲ ਦੇ ਅਟੱਲ ਨੁਕਸਾਨ 5% ਤੋਂ ਵੱਧ ਨਹੀਂ ਹੁੰਦੇ ਹਨ। · ਲੰਬਾਈ ਅਤੇ ਵਿਆਸ ਅਤੇ ਵਾਤਾਵਰਣ ਕਾਰਕਾਂ ਦੇ ਅਨੁਪਾਤ ਦੇ ਕਾਰਨ ਚੁੰਬਕ ਦਾ ਵੱਧ ਤੋਂ ਵੱਧ ਕਾਰਜਸ਼ੀਲ ਤਾਪਮਾਨ ਬਦਲਿਆ ਜਾ ਸਕਦਾ ਹੈ। . |
ਫਾਇਦਾ:
ਇਹਨਾਂ ਚੁੰਬਕਾਂ ਦੀਆਂ ਵਿਸ਼ੇਸ਼ਤਾਵਾਂ ਰਵਾਇਤੀ ਨਾਲੋਂ ਕਿਤੇ ਉੱਚੀਆਂ ਹਨ ਅਤੇ ਇਹ ਵਰਤਮਾਨ ਵਿੱਚ ਉਪਯੋਗ ਵਿੱਚ ਸਭ ਤੋਂ ਸ਼ਕਤੀਸ਼ਾਲੀ ਹਨ। ਉਨ੍ਹਾਂ ਦੇ ਉੱਚ
ਜਬਰਦਸਤੀ ਅਤੇ ਉੱਚ ਰਹਿਤਤਾ ਨਵੇਂ ਡਿਜ਼ਾਈਨ ਅਤੇ ਐਪਲੀਕੇਸ਼ਨ ਦੇ ਚੁੰਬਕੀ ਖੇਤਰ ਨੂੰ ਵਧਾਉਣ ਦੀ ਸੰਭਾਵਨਾ ਦੀ ਆਗਿਆ ਦਿੰਦੀ ਹੈ ਜਿੱਥੇ ਸਪੇਸ ਸੀਮਤ ਹੈ
ਜਾਂ ਜਿੱਥੇ ਇੱਕ ਮਜ਼ਬੂਤ ਚੁੰਬਕੀ ਖੇਤਰ ਦੀ ਲੋੜ ਹੁੰਦੀ ਹੈ।
NdFeB ਮੈਗਨੇਟ ਖੋਰ ਲਈ ਬਹੁਤ ਸੰਵੇਦਨਸ਼ੀਲ ਹੁੰਦੇ ਹਨ। ਇਸ ਲਈ ਇੱਕ ਸੁਰੱਖਿਆ ਸਤਹ ਪਰਤ ਦੀ ਲੋੜ ਹੈ. NdFeB ਚੁੰਬਕ ਦੀਆਂ ਵਰਤੋਂ ਕੰਡੀਸ਼ਨਡ ਹਨ
80ºC ਤੋਂ 230ºC ਤੱਕ ਚੱਲਣ ਵਾਲੀ ਇੱਕ ਵਿਆਪਕ ਰੇਂਜ ਵਿੱਚ ਤਾਪਮਾਨ ਦੁਆਰਾ। ਅਤੇ ਇਹ 0 ℃ ਤੋਂ ਘੱਟ ਤਾਪਮਾਨ ਤੇ ਵੀ ਕੰਮ ਕਰਦਾ ਹੈ.
ਐਪਲੀਕੇਸ਼ਨ:
ਨਿਓਡੀਮੀਅਮ ਮੈਗਨੇਟ ਨੂੰ ਫੋਕਸ ਕਰਨ, ਇਲੈਕਟ੍ਰੋਨਿਕਸ ਵਿੱਚ ਚਾਰਜ ਕੀਤੇ ਕਣਾਂ ਦੇ ਵਿਗਾੜ, ਬ੍ਰੇਕ ਸਿਸਟਮ,
ਡ੍ਰਿੱਪ, ਸੈਂਸਰ, ਰੋਟਰ ਅਤੇ ਮਾਈਕ੍ਰੋ ਮੋਟਰਾਂ ਵਿੱਚ ਚੁੰਬਕੀ ਪ੍ਰਣਾਲੀ, ਅਤੇ ਵਿਗਿਆਨ, ਦਵਾਈ (ਟੋਮੋਗ੍ਰਾਫੀ, NMR ਸਪੈਕਟਰੋਮੀਟਰ), ਆਦਿ ਦੇ ਖੇਤਰ।
ਅੱਜ, ਪੂਰੀ ਦੁਨੀਆ ਵਿੱਚ NdFeB ਮੈਗਨੇਟ ਵੱਡੀ ਮਾਤਰਾ ਵਿੱਚ ਵਰਤੇ ਜਾਂਦੇ ਹਨ। ਇਸ ਸਮੱਗਰੀ ਦਾ ਵਿਕਾਸ ਅਜੇ ਪੂਰਾ ਨਹੀਂ ਹੋਇਆ ਹੈ; remanence
ਅਤੇ ਜ਼ਬਰਦਸਤੀ ਖੇਤਰ ਦੀ ਤਾਕਤ ਨੂੰ ਲਗਾਤਾਰ ਵਧਾਇਆ ਜਾ ਰਿਹਾ ਹੈ। NdFeB ਮੈਗਨੇਟ ਦੀ ਉੱਚ ਊਰਜਾ ਦਾ ਮਤਲਬ ਹੈ ਕਿ ਮੋਟਰਾਂ ਅਤੇ ਸੈਂਸਰ ਬਣਾਏ ਜਾ ਸਕਦੇ ਹਨ
ਕਦੇ ਵੀ ਛੋਟਾ - ਅਤੇ ਇਹ ਪ੍ਰਦਰਸ਼ਨ ਕੁਸ਼ਲਤਾ ਵਿੱਚ ਵਾਧਾ ਦਰਸਾਉਂਦਾ ਹੈ। ਚੱਲ ਰਹੇ ਸੁਧਾਰ ਇਸ ਦਿਲਚਸਪ ਸਮੱਗਰੀ ਨੂੰ ਨਿਰੰਤਰ ਹੋਣ ਦੇ ਯੋਗ ਬਣਾਉਂਦੇ ਹਨ-
ਨਵੇਂ ਖੇਤਰਾਂ ਵਿੱਚ ਆਮ ਤੌਰ 'ਤੇ ਪੇਸ਼ ਕੀਤਾ ਜਾਂਦਾ ਹੈ।
ਸਾਰੇ ਦੱਸੇ ਗਏ ਮੁੱਲ IEC 60404-5 ਦੇ ਅਨੁਸਾਰ ਮਿਆਰੀ ਨਮੂਨਿਆਂ ਦੀ ਵਰਤੋਂ ਕਰਕੇ ਨਿਰਧਾਰਤ ਕੀਤੇ ਗਏ ਸਨ। ਹੇਠ ਲਿਖੀਆਂ ਵਿਸ਼ੇਸ਼ਤਾਵਾਂ ਸੰਦਰਭ ਮੁੱਲਾਂ ਵਜੋਂ ਕੰਮ ਕਰਦੀਆਂ ਹਨ ਅਤੇ
ਵੱਖਰਾ ਹੋ ਸਕਦਾ ਹੈ। ਵਧੇਰੇ ਜਾਣਕਾਰੀ ਲਈ ਕਿਰਪਾ ਕਰਕੇ ਸਾਡੇ ਐਪਲੀਕੇਸ਼ਨ ਇੰਜੀਨੀਅਰਾਂ ਨਾਲ ਸੰਪਰਕ ਕਰੋ।